wood, douglas fir (#891)
ID-number | #891 |
---|---|
Material | wood, douglas fir |
Classification | ECN Phyllis classification ▸ untreated wood ▸ fir/pine/spruce ▸ wood, douglas fir |
NTA 8003 classification ▸ [100] hout ▸ [110] vers hout ▸ [130] naaldhout ▸ [131] naaldhout | |
Sample lot size | mesh -4+16 |
Submitter organisation | ECN (Netherlands) |
Remarks | hog fuel |
Literature | R. J. Evans, A. R. Knight, M. Onischak and S. P. Babu: Development of biomass gasification to produce substitute fuels, Richland, Washington, USA, Pacific Northwest Laboratory (PNL), PNL--6518, 14 p. (1988). |
Values
Property | Unit | Value | Std dev | Det lim | Lab | Date | Method | Remarks | ||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
ar | dry | daf | ||||||||||||||||||
Main biomass properties |
||||||||||||||||||||
Ash melting behaviour |
||||||||||||||||||||
American standard method, measured in oxidizing conditions |
||||||||||||||||||||
IDT (initial deformation temperature) | °C | 1 177 | ||||||||||||||||||
SOT (softening or spherical temperature) | °C | 1 257 | ||||||||||||||||||
HT (hemispherical temperature) | °C | 1 360 | ||||||||||||||||||
FT (fluid temperature) | °C | 1 463 | ||||||||||||||||||
American standard method, measured in reducing conditions |
||||||||||||||||||||
IDT (initial deformation temperature) | °C | 1 132 | ||||||||||||||||||
SOT (softening or spherical temperature) | °C | 1 201 | ||||||||||||||||||
HT (hemispherical temperature) | °C | 1 279 | ||||||||||||||||||
FT (fluid temperature) | °C | 1 354 | ||||||||||||||||||
Physical Properties |
||||||||||||||||||||
Commonly used properties |
||||||||||||||||||||
Bulk density (ar) | kg/m³ (ar) | 210 |