wood, willow, 5-9 mm (#886)

ID-number#886
Materialwood, willow, 5-9 mm
Classification ECN Phyllis classification ▸ untreated wood ▸ willow
NTA 8003 classification ▸ [100] hout ▸ [110] vers hout ▸ [120] loofhout ▸ [122] zacht loofhout
Ash typeISO 1171 (815 degC)
Submitter organisationECN (Netherlands)
Remarkstested in ECN CFB gasifier (BIVKIN)
LiteratureJ. W. Vermeulen and A. van der Drift: Brandstoffen uit reststromen voor circulerend wervelbedvergassing, rapportage fase 2, (non-confidential version, in Dutch), Haarlem, NV Afvalzorg (1998).

Values

Property Unit Value Std dev Det lim Lab Date Method Remarks
ar dry daf

Main biomass properties

Proximate analysis

Moisture content wt% 17.00

Trace elements composition

Arsenic (As) mg/kg (dry) 1.0
Calcium (Ca) mg/kg (dry) 5 700.0 Measured
Cadmium (Cd) mg/kg (dry) 2.4 Measured
Cobalt (Co) mg/kg (dry) 0.6 Measured
Chromium (Cr) mg/kg (dry) 14.0 Measured
Copper (Cu) mg/kg (dry) 13.0 Measured
Iron (Fe) mg/kg (dry) 68.0 Measured
Mercury (Hg) mg/kg (dry) 0.1 Measured
Potassium (K) mg/kg (dry) 2 500.0 Measured
Magnesium (Mg) mg/kg (dry) 520.0 Measured
Manganese (Mn) mg/kg (dry) 10.0 Measured
Sodium (Na) mg/kg (dry) 180.0 Measured
Nickel (Ni) mg/kg (dry) 26.0 Measured
Phosphorus (P) mg/kg (dry) 710.0 Measured
Lead (Pb) mg/kg (dry) 240.0 Measured
Antimony (Sb) mg/kg (dry) 1.0
Selenium (Se) mg/kg (dry) 1.0
Silicon (Si) mg/kg (dry) 620.0 Measured
Tin (Sn) mg/kg (dry) 1.7 Measured
Tellurium (Te) mg/kg (dry) 1.0
Vanadium (V) mg/kg (dry) 0.3 Measured
Zinc (Zn) mg/kg (dry) 97.0 Measured

Physical Properties

Commonly used properties

Bulk density (ar) kg/m³ (ar) 170