wood, oak, swamp (#307)
ID-number | #307 |
---|---|
Material | wood, oak, swamp |
Classification | ECN Phyllis classification ▸ untreated wood ▸ oak ▸ wood, oak, swamp |
NTA 8003 classification ▸ [100] hout ▸ [110] vers hout ▸ [120] loofhout ▸ [125] hard loofhout | |
Submitter organisation | ECN (Netherlands) |
Literature | H. F. Feldmann, M. A. Paisley, H. R. Appelbaum and D. R. Taylor: Conversion of forest residues to a methane-rich gas in a high-throughput gasifier, Battelle, Columbus, OH (USA), DE88013138, 108 p. (1988). |
Values
Property | Unit | Value | Std dev | Det lim | Lab | Date | Method | Remarks | ||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
ar | dry | daf | ||||||||||||||||||
Main biomass properties |
||||||||||||||||||||
Proximate analysis |
||||||||||||||||||||
Moisture content | wt% | 5.50 | ||||||||||||||||||
Ash content | wt% | 0.94 | 0.99 | |||||||||||||||||
Volatile matter | wt% | 79.69 | 84.33 | 85.17 | ||||||||||||||||
Fixed carbon | wt% | 13.87 | 14.68 | 14.83 | Calculated | |||||||||||||||
Ultimate analysis (macroelements) |
||||||||||||||||||||
Carbon | wt% | 46.96 | 49.69 | 50.19 | Measured | |||||||||||||||
Hydrogen | wt% | 5.98 | 6.33 | 6.39 | Measured | |||||||||||||||
Oxygen | wt% | 40.48 | 42.84 | 43.27 | Calculated | |||||||||||||||
Nitrogen | wt% | 0.12 | 0.13 | 0.13 | Measured | |||||||||||||||
Sulphur | wt% | 0.00 | 0.00 | 0.00 | Measured | |||||||||||||||
Total (with halides) | wt% | 100.00 | 100.00 | 100.00 | Calculated | |||||||||||||||
Halides |
||||||||||||||||||||
Chlorine (Cl) | mg/kg | 189.0 | 200.0 | 202.0 | Measured | |||||||||||||||
Heating value |
||||||||||||||||||||
Net calorific value (LHV) | MJ/kg | 17.16 | 18.30 | 18.49 | ||||||||||||||||
Gross calorific value (HHV) | MJ/kg | 18.60 | 19.68 | 19.88 | ||||||||||||||||
HHVMilne | MJ/kg | 19.03 | 20.14 | 20.34 | Calculated |