sugarcane bagasse pyrolysis oil (#2343)

ID-number#2343
Materialsugarcane bagasse pyrolysis oil
Classification ECN Phyllis classification ▸ others ▸ non-fossil oil
NTA 8003 classification ▸ [800] samengestelde stromen ▸ [802] brandstof na pyrolyse
Submitter organisationECN (Netherlands)
Submission date2003-03-25
Remarksproduced at 530°C by vacuum pyrolysis. pH 2.7, flash point >90°C
LiteratureM. Garcìa-Pèrez, A. Chaala, C. Roy: Vacuum pyrolysis of sugarcane bagasse. J. Anal. Appl. Pyrolysis 65 (2002)111-136.

Values

Property Unit Value Std dev Det lim Lab Date Method Remarks
ar dry daf

Fuel Properties

Proximate Analysis

Moisture content wt% 13.80
Ash content wt% 0.04 0.05

Ultimate Analysis

Carbon wt% 47.07 54.60 54.63 Measured
Hydrogen wt% 5.56 6.45 6.45 Measured
Nitrogen wt% 0.63 0.73 0.73 Measured
Sulphur wt% (dry) 0.10
Oxygen wt% 32.82 38.07 38.09 Calculated
Total (with halides) wt% 99.91 99.90 99.90 Calculated

Calorific Values

Net calorific value (LHV) MJ/kg 20.85 24.58 24.59
Gross calorific value (HHV) MJ/kg 22.40 25.99 26.00
HHVMilne MJ/kg 19.39 22.49 22.50 Calculated

Chemical Analyses

Major elements

Aluminium (Al) mg/kg (dry) 10.1 Measured
Potassium (K) mg/kg (dry) 5.3 Measured
Sodium (Na) mg/kg (dry) 21.5 Measured
Calcium (Ca) mg/kg (dry) 33.8 Measured
Magnesium (Mg) mg/kg (dry) 2.2 Measured
Iron (Fe) mg/kg (dry) 105.8 Measured
Phosphorus (P) mg/kg (dry) 3.3 Measured
Titanium (Ti) mg/kg (dry) 0.2 Measured

Minor elements

Cobalt (Co) mg/kg (dry) 0.1 Measured
Chromium (Cr) mg/kg (dry) 0.6 Measured
Copper (Cu) mg/kg (dry) 2.3 Measured
Manganese (Mn) mg/kg (dry) 1.1 Measured
Nickel (Ni) mg/kg (dry) 1.1 Measured
Lead (Pb) mg/kg (dry) 4.9 Measured
Vanadium (V) mg/kg (dry) 0.0 Measured
Zinc (Zn) mg/kg (dry) 43.7 Measured
Selenium (Se) mg/kg (dry) 0.2 Measured

Other elements

Antimony (Sb) mg/kg (dry) 7.7 Measured

Physical Properties

Commonly used properties

Bulk density (ar) kg/m³ (ar) 1 211