Japanese larch, karamatsu (#2279)
ID-number | #2279 |
---|---|
Material | Japanese larch, karamatsu |
Classification | ECN Phyllis classification ▸ untreated wood ▸ other soft wood |
NTA 8003 classification ▸ [100] hout ▸ [110] vers hout ▸ [130] naaldhout ▸ [131] naaldhout | |
Submitter organisation | ECN (Netherlands) |
Submission date | 2002-08-05 |
Remarks | holocellulose 69.5%, ethanol-benzene solubles 0.9%; see also Y. Kurimoto et al., Holzforschung 53 (1999) 617-622: 1% NaOH soluble 16.6% |
Literature | Y. Kurimoto, A. Koizumi, S. Doi, Y. Tamura, H. Ono: Wood species effects on the characteristics of liquefied wood and the properties of polyurethane films prepared from the liquefied wood. Biomass and Bioenergy 21 (2001) 381-390. |
Values
Property | Unit | Value | Std dev | Det lim | Lab | Date | Method | Remarks | ||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
ar | dry | daf | ||||||||||||||||||
Main biomass properties |
||||||||||||||||||||
Proximate analysis |
||||||||||||||||||||
Moisture content | wt% (ar) | |||||||||||||||||||
Ash content | wt% | 0.20 | ||||||||||||||||||
Ultimate analysis (macroelements) |
||||||||||||||||||||
Total (with halides) | wt% | 0.20 | 0.00 | Calculated | ||||||||||||||||
Biochemical analysis |
||||||||||||||||||||
Cellulose, hemicellulose, lignin |
||||||||||||||||||||
Lignin | wt% (dry) | 22.50 | Measured | |||||||||||||||||
Other |
||||||||||||||||||||
Extractives EtOH/toluene | wt% (dry) | 0.90 | Measured | |||||||||||||||||
Extractives hot water | wt% (dry) | 6.90 | Measured | |||||||||||||||||
Total ash + biochemical | wt% (dry) | 30.50 | Calculated |